Complete Tender Details

Empowering Indian businesses in the procurement ecosystem since 2012

Tendering Authority: Visakhapatnam Port Trust
Tender ID3579916
Organisation NameVisakhapatnam Port Trust
Tender BriefCorrigendum : Repairs To The Structural Components Of Wq 1,2,3 Berths, Kerb Walls And Drains In The Backup Area
Last Date For Submission13th Apr, 2026
Opening Date15 Apr, 2026
Cost
Document Cost1770.00
EMD381550.00
Estimated Cost28154250.00
Location
CityMulti city
StateMulti State

Register to see full details

BOQ Items
#ItemQtyUnits
1Working plat Form: The working platform above the water level shall be erected using the friction support from adjacent two piles and hanging support from the top of the deck. The above fixing and erection work shall be carried out with the help of floating pontoon and boats etc. Providing, erecting and dismantling safe scaffolding including working platform for external and internal area to facilitate all works with proper arrangements etc. complete. The cost of equipment, plants, materials, sand, instrumentation, hiring of boat, catamaran, pontoon,labour and survey,fuel etc.., as required and as directed by the Engineer-in-charge complete. All labour and materials.1106.001m2
2Surface Preparation: Labour charges for chipping the spalled and old concrete of the RC Structural Element. Check for the phenolphthalein test and if there is no change in color, chip the same further down until, reaching the good or uncontaminated concrete. Clean the surface and make sure that surface is clean and free from loose particles. The rate shall include cost of equipment, plants, instrumentation, hiring of boat, catamaran, pontoon, labour and survey, fuel etc. Engineer-in-charge complete. All labour and materials.20281m2
3Shear Connectors: Drilling 12mm diameter holes up to a depth of 75mm maximum and fixing 8mm diameter L- shaped anchor rods as shear connectors at every 500mm c/c on the surfaces of the Pile or any other structural member, as the case may be. Clean the same using water and make sure that there are no fine particles present in the hole. Mix the base and hardener of the polyester resin, like Lokfix S/P manufactured by Fosroc or equivalent, thoroughly with the spatula. Fill the drilled and cleaned holes to a minimum depth of 1/3rd of the hole with the prepared polyester resin. Make sure that the resin has reached till the end of the hole. At this stage, push the shear connector gently into the hole and finish the excess resin which comes out of the hole, and allow the shear connectors not to be disturbed for a minimum of 20 minutes -complete. The cost of equipment, plants, materials, sand, instrumentation, hiring of boat, catamaran, pontoon,labour and survey,fuel etc.., as required and as directed by the Engineer-in-charge complete. All labour and materials. 8114Each
4Provision of Galvanic Anode: Before installation of the self-sacrificial anode Galvashield XPI manufactured by Vector Technologies or equivalent, check the continuity of the steel reinforcement. Any loss of continuity will require additional electrical connections or restoration of continuity by effective means. Select a location for the Galvashield XPI or equivalent as close as practical to the edge of the repair zone. Galvashield XPI units should be positioned around/along the repair boundary. In addition to standard substrata preparation, the Galvashield XPI anode(s) shall be thoroughly pre-soaked in clean water for a minimum of 10 minutes and a maximum of 20 mintues prior to the application of the repair mortar. Tighten tie wires using the Galvashield fixing Tool so that no free movement is possible, thus ensuring good electrical continuity. To test electrical continuity between tie wires and reinforcement bar, a continuity meter like an electrical multimeter should be used. The rate shall include the cost of equpiment, plants, materials, instrumentation, hiring of boat,catamaran,ponoon,labour and survey,fuel etc.., as required and as directed by the Engineer-in-charge complete.All labour and materials.2028Each
5Anti-corrosive Coating: Clean the rebars using the rust remover if there exists any rust, otherwise clean the rebar free of foregin material followed by Clean reinforcement using Reebaklens RR of Fosroc or equivalent; otherwise, clean the rebar free of foreign material. Mix the base and hardener of the anti- corrosive coating like Nitozinc Primer of Fosroc or equivalent, mechanically using a slow-speed, heavy-duty drilling machine fitted with a mixing paddle. Apply the mixed materials to the cleaned rebar at 45 microns/coat and total dry film thickness (DFT 90) microns in 2 coats and allow it to dry completely. The rate shall include the cost of equipment, plants, materials, instrumentation,hiring of boat ,catamaran,ponoon,labour and survey,fuel etc.., as required and as directed by the Engineer-in-charge complete.All labour and materials.255Ltr